Velo3D qualifies new Haynes superalloy for Sapphire printers

Stay up to date with everything that is happening in the wonderful world of AM via our LinkedIn community.

Velo3D, an expert metal additive manufacturing technology company for mission-critical parts, has qualified the nickel-based superalloy powder Amperprint 0233 Haynes 282 for use in its Sapphire family of printers. The powder was produced by Höganäs AB under license from Haynes International and is designed for high creep strength, thermal stability, weldability, and fabricability not commonly found in other alloys. The material is ideal for high-temperature structural applications like energy generation, gas turbines, and space launch vehicles to build parts like heat exchangers, combustors, nozzles, combustion liners, rocket engines, and shrouded impellers.

The first Sapphire printer utilizing the Amperprint 0233 Haynes 282 powder will be operated by Duncan Machine Products (DMP), a contract manufacturer based in Duncan, Oklahoma. The system will be the seventh in DMP’s fleet of Velo3D Sapphire printers.

Velo3D has qualified the nickel-based superalloy powder Amperprint 0233 Haynes 282 for use in its Sapphire family of printers

“Our goal at Velo3D is to enable engineers to build the parts they want without compromising on the design or quality,” said Benny Buller, Velo3D CEO and Founder. “Qualifying new powdered metals, like Amperprint 0233 Haynes 282, for use in our end-to-end solution, further expands what’s possible with our additive manufacturing technology. Our partners at Höganäs provide materials of the highest quality, and I look forward to seeing what our customers build using this amazing alloy.”

Haynes 282 alloy (see all material data) is available in a full range of product forms and sizes, including plate, sheet and coil products from foil thickness up to cross-sections greater than 2” (>50mm) thick; Bar and wire from up to 9” in diameter, Reforge billet and ingot products from 4” up to 20” (100-500mm) diameters; and seamless and welded Pipe and tube in some standard sizes. Vacuum castings have also been produced for various applications, and powder products are available to support many Additive Manufacturing methods.

Powdered nickel-based superalloys, like Amperprint 0233 Haynes 282, are often used to print parts for use in high-temperature applications due to the alloy’s resistance to cracking and its ability to operate at near-melting-point temperatures. This tolerance allows parts printed with the alloy to be used in vacuum, plasma, and other demanding applications. Its high weldability makes the powder ideal for parts in larger systems because of its ability to be welded to other components. Höganäs specializes in creating powders for additive manufacturing, delivering products with a consistent spherical shape, tight control on chemistry, and enhanced flowability. The powders are made using the purest materials with very precise compositions of trace elements that give the metals their unique properties.

Velo3D has qualified the nickel-based superalloy powder Amperprint 0233 Haynes 282 for use in its Sapphire family of printers

“It’s inspiring to see what engineers have been able to build using metal powders from Höganäs and Velo3D’s support-free additive manufacturing process,” said Jerome Stanley, Höganäs Director of Global Sales, Customization Technologies. “The first parts printed using our Amperprint 0233 Haynes 282 powder is impressive, and I believe customers are only scratching the surface of what is possible with this superalloy. The powder, combined with Velo3D’s end-to-end solution metal AM solution, is an extremely effective combination for consolidating parts into monolithic structures to eliminate coefficient of thermal expansion in large, high-performance systems.” Velo3D is one of the first additive manufacturing technology companies to offer Amperprint 0233 Haynes 282 powder to its customers. Many of Velo3D’s customers use its end-to-end solution to produce parts for use in aviation, energy, oil and gas, space, and other high-performance applications, making the powder a good fit for Velo3D’s portfolio. In addition to Amperprint 0233 Haynes 282 powder, metal powders qualified to be printed with Velo3D’s technology include Hastelloy X, Inconel 718, aluminum F357, Ti 6Al-4V Grade 5, and several additional materials.

Research
Consumer Products AM 2024

This new market study from VoxelMatters provides an in-depth analysis and forecast of polymer and metal AM in the consumer products industry across the three core segments of the additive manufactu...

Related Articles

Leave a Reply

Your email address will not be published. Required fields are marked *

Back to top button
Close Popup
Privacy Settings saved!
Privacy Settings

When you visit any web site, it may store or retrieve information on your browser, mostly in the form of cookies. Control your personal Cookie Services here.

These cookies are necessary for the website to function and cannot be switched off in our systems.

Technical Cookies
In order to use this website we use the following technically required cookies
  • PHPSESSID
  • wordpress_test_cookie
  • wordpress_logged_in_
  • wordpress_sec

Decline all Services
Save
Accept all Services

Newsletter

Join our 12,000+ Professional community and get weekly AM industry insights straight to your inbox. Our editor-curated newsletter equips executives, engineers, and end-users with crucial updates, helping you stay ahead.